Improving inspection methods
Not to be implemented
Rail R
Accident
17.11.2000
C14/1999R/S138
Recommendation
The rail inspection methods should be developed also to permit an early detection of beginning vertical ruptures (capillary cracks) along the rail. Rails displaying surface defects (flakes) should be repaired as soon as possible so as to allow a reliable ultrasonic measurement of the rail condition.
Investigation report
C14/1999R Tank wagon derailing in Hamina port, on 19 September, 1999